HS 252329
Oil well cement API Class H HSR
API 10A Class H high sulphate resistant basic well cement for deep and hot wells, mixed at 38 % water; bulk, sacks or big bags.

Specifications
| HS code | 252329 |
|---|---|
| Standard | API Spec 10A / ISO 10426-1 Class H, HSR |
| C3S / C3A | 48-65 % / ≤ 3 % |
| MgO / SO3 | ≤ 6.0 % / ≤ 3.0 % |
| Mixing water | 38 % by weight of cement |
| Free fluid | ≤ 5.9 % |
| 8 h compressive strength at 38 °C | ≥ 2.1 MPa (300 psi) |
| Packing | Bulk, 1.5 t big bags or 94 lb (42.6 kg) sacks; 20' container or bulk vessel |
| Typical origins | Türkiye, China |
What sets the price
- Sea freight and vessel size: handysize, supramax or container
- Kiln fuel cost: coal and petcoke prices
- EU CBAM pushing Mediterranean exporters toward Africa, the US and the Levant
- Domestic demand in Egypt and Vietnam that tightens export supply